- [English]
- The Formation and Crystallization of Amorphous Ti50Cu50Ni20Al10 Powder Prepared by High-Energy Ball Milling
-
Nguyen Hoang Viet, Jin-Chun Kim, Ji-Soon Kim, Young-Soon Kwon
-
J Korean Powder Metall Inst. 2009;16(1):9-15.
-
DOI: https://doi.org/10.4150/KPMI.2009.16.1.009
-
-
264
View
-
0
Download
-
1
Citations
-
Abstract
PDF
- Amorphization and crystallization behaviors of Ti_50Cu_50Ni_20Al_10 powders during high-energy ball milling and subsequent heat treatment were studied. Full amorphization obtained after milling for 30 h was confirmed by X-ray diffraction and transmission electron microscope. The morphology of powders prepared using different milling times was observed by field-emission scanning electron microscope. The powders developed a fine, layered, homogeneous structure with prolonged milling. The crystallization behavior showed that the glass transition, T_g, onset crystallization, T_x, and super cooled liquid range DeltaT=T_x-T_g were 691,771 and 80 K, respectively. The isothermal transformation kinetics was analyzed by the John-Mehn-Avrami equation. The Avrami exponent was close to 2.5, which corresponds to the transformation process with a diffusion-controlled type at nearly constant nucleation rate. The activation energy of crystallization for the alloy in the isothermal annealing process calculated using an Arrhenius plot was 345 kJ/mol.
-
Citations
Citations to this article as recorded by 
- Mechanical Properties of Bulk Amorphous Ti50Cu20Ni20Al10Fabricated by High-energy Ball Milling and Spark-plasma Sintering
H.V. Nguyen, J.C. Kim, J.S. Kim, Y.J. Kwon, Y.S. Kwon Journal of Korean Powder Metallurgy Institute.2009; 16(5): 358. CrossRef
|