This is an Open-Access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/3.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.
NO. | Substrate | Binder | Temperature | Area (cm2) | VMAX (V) | VOC (V) | JSC (mA/cm2) | FF | Efficiency (%) |
---|---|---|---|---|---|---|---|---|---|
|
|||||||||
1 | FTO Glass | Organic | 450°C | 0.25 | 0.4159 | 0.5638 | 10.30 | 0.6212 | 3.607 |
2 | Peroxo titanium complex | 450°C | 0.4635 | 0.5981 | 7.746 | 0.6860 | 3.178 | ||
3 | 400°C | 0.4658 | 0.5902 | 5.175 | 0.7028 | 2.147 | |||
4 | 300°C | 0.4287 | 0.5672 | 5.182 | 0.6461 | 1.899 | |||
5 | 150°C | 0.4366 | 0.5773 | 3.878 | 0.6531 | 1.462 |