Abstract
The microstructure and hardness of (W,Ti)C cemented carbides with a different metallic binder composition of Ni and Co fabricated by powder technology were investigated. The densifications of the prepared materials were accomplished by using vacuum sintering at 1450°C. Nearly full dense (W,Ti)C cemented carbides were obtained with a relative density of up to 99.7% with 30 wt.% Co and 99.9% with 30 wt.% Ni as a metallic binder. The average grain size of the (W,Ti)C-Co and the (W,Ti)C-Ni was decreased by increasing the metallic binder content. The hardness of the dense (W,Ti)C-15 wt%Co and (W,Ti)C-15 wt%Ni, was greater than that of the other related cemented carbides; in addition, the cobalt-based cemented carbides had greater hardness values than the nickel-based cemented carbides.
Citations
Citations to this article as recorded by

- Performance Evaluation on the Endmill of High Speed Machining for Selection of Tungsten Carbide (WC-Co) Material
Dong-Hee Kwon, Jeong-Suk Kim, Min-Wook Kim, Young-Keun Jeong, Myung-Chang Kang
Journal of Korean Powder Metallurgy Institute.2008; 15(5): 359. CrossRef